ILT-U-313
Tension testing of steel wire
DETERMINATION | METHOD |
| Ultimate tensile strength in MPa | ASTM E8 |
| Yield strength offset = 0,2% in MPa | ASTM E8 |
| Elongation in % | ASTM E8 |
| Reduction of area in % | ASTM E8 |


Tension testing of steel wire
DETERMINATION | METHOD |
| Ultimate tensile strength in MPa | ASTM E8 |
| Yield strength offset = 0,2% in MPa | ASTM E8 |
| Elongation in % | ASTM E8 |
| Reduction of area in % | ASTM E8 |