ILT-U-3978
Determinations for 3-Layer Polyethylene (3LPE) Coatings
DETERMINATION | METHOD |
| Impact Test | ISO 21809-1:2018 Annex E |
| Hot Water Immersion Test (Test conditions: Temperature: 80 °C; Duration: 48 hours) | ISO 21809-1:2018 Annex L |
| Thermal analysis of epoxy and cured epoxy coating film (Measurements: Tg3, Tg4, ΔTg, ΔH1 and C) | ISO 21809-1:2018 Annex D |